http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101462656-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K30-35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2387-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-883 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-565 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 |
filingDate | 2008-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101462656-B1 |
titleOfInvention | Method for producing nanoparticle / block copolymer complex |
abstract | The present invention relates to a method for preparing a nanoparticle / block copolymer composite, and more particularly, to a nanoparticle / block copolymer composite comprising nanoparticles containing an organic ligand (L); (AbB) containing block repetition units (A, B) having different solubility parameters are mixed in a solvent (S) to form a micelle by self-assembly, and the step Organic ligands (L); A block copolymer (A-b-B) comprising block repeat units (A, B); And a solubility parameter (?) Of the solvent (S) satisfy the following equations (1) to (3), it is possible to provide a method for producing a nanoparticle / , The chemical and mechanical properties can be maintained or improved.n n n [Equation 1]n n n 29 ≤ δ S - δ A n n n &Quot; (2) "n n n δ S - δ B ≤ 29n n n &Quot; (3) "n n n | 隆 L - 隆 A | ? 5, or |? L -? B | ≤ 5n n n (In the above formulas 1 to 3, 隆 S is the solubility parameter of the solvent, 隆 A is the solubility parameter of the block repeating unit A, 隆 B is the solubility parameter of the block repeating unit B, and 隆 L is the solubility parameter of the ligand to be.)n n n n Nanoparticle, block copolymer, micelle, solubility parameter |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220097282-A |
priorityDate | 2008-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 81.