Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-0062 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B11-0282 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-147 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B11-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B11-007 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B11-028 |
filingDate |
2007-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2014-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101432334-B1 |
titleOfInvention |
Calcium sulfate halide treatment process |
abstract |
The present invention relates to a process for treating beta calcium sulfate hemihydrate. The process comprises exposing the beta calcium sulfate hemi-hydrate to steam at a pressure above atmospheric pressure.n n n n Gypsum, Beta calcium sulfate, Half-hydrate, Water requirement |