http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101423123-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3f60ec912f2e8b214477769b5e970ae5 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02D31-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02D3-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B09B1-008 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E02D31-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B1-00 |
filingDate | 2014-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c984de1d6896f8be6ab927bd914df43d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecc9e94c9c191b6516efef5ef10b8954 |
publicationDate | 2014-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101423123-B1 |
titleOfInvention | Method for constructing impervious wall of waste landfill pond |
abstract | The present invention relates to a method for constructing a wastewater landfill composition for soil composition, in which a solidifying agent is sprayed in accordance with an optimum water content for accelerating cementation and strength enhancement of mixed soil, and cracks are not generated during the curing process. In order to accomplish the above object, there is provided a method for constructing a wastewater landfill composition for a landfill according to the present invention, comprising the steps of: (S20) preparing mottos so as to remove the impurities from the soil containing impurities such as stones and foreign matter; (S30) of forming a reinforcing layer on the bottom and slopes by mixing Portland cement and soil stabilizer with some of the prepared mottos; (S40) of constructing an aeration layer above the bottom surface of the reinforcing layer, wherein the aeration layer construction step (S40) comprises 10 to 15 parts by weight of ordinary Portland cement and 3 to 5 parts by weight of bentonite with respect to 100 parts by weight of the prepared mortar Forming a solidification mixture (S41); (S42) preparing 1 to 5 parts by weight of a solidifying agent aqueous solution based on the weight of the above-mentioned grounding agent, and uniformly spraying said solidifying agent aqueous solution to said solidifying mixed soil using a high-pressure atomizer; A step (S43) of evenly shaping the aquedient layered solidified soil mixed with the solidifying agent solution sprayed on the upper part of the reinforcing layer formed on the bottom surface; A step of compiling a solidified aquifer-shaped solidified soil (S44); And a step (S45) of curing for a certain period of time after compaction. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112281926-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112281926-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101717693-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101717689-B1 |
priorityDate | 2014-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 33.