http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101410066-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08782 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0821 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0806 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08795 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2010-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101410066-B1 |
titleOfInvention | Electrostatic image developing toner |
abstract | The present invention relates to a resin composition comprising a binder resin; coloring agent; And an amount of absorbance derived from the binder resin at 828 cm < -1 > at 2,850 cm < -1 & gt ;, which is expressed by "absorbance derived from wax / Wherein the intensity ratio is measured by measuring the amount of wax present at a depth of 0.3 mu m or less from the surface of the toner particles after heating the toner to 140 DEG C and then cooling it, wherein the intensity ratio is measured by FTIR- Wherein the toner has a storage elastic modulus at 140 占 폚 of 5,000 Pa or more. |