Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-0095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48137 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2933-0075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2933-0066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L25-0753 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-48091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F21V19-003 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-644 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-647 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L24-97 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-64 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L33-48 |
filingDate |
2012-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101400271-B1 |
titleOfInvention |
Optical device manufacturing method and optical device manufactured thereby |
abstract |
The present invention relates to a method of manufacturing an optical device that improves heat dissipation performance through a heat sink and insulation performance between the substrate and the heat sink, and improves workability, and an optical device manufactured thereby. According to a first aspect of the present invention, there is provided a method of manufacturing an optical device, comprising: (a) preparing an original plate for an optical device having a vertical insulating layer; (B) forming a thickness groove along a cutting line on a bottom surface of the original plate for the optical device; (C) forming an electric insulating layer having a flat surface by applying a liquid insulating material to the surface having the grooves formed thereon and curing the surface, and (c) forming a fixing hole penetrating the optical device main plate and the thickness grooves both up and down d). |