http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101367952-B1

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F27-292
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F17-0033
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-9615
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-77
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3284
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3281
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5445
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2237-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2237-346
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F17-0013
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B18-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F3-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F41-046
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-462
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G23-003
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G4-30
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G4-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-462
filingDate 2012-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2014-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2014-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-101367952-B1
titleOfInvention Nonmagnetic composition for laminated electronic component, laminated electronic component using same and manufacturing method thereof
abstract The present invention relates to a nonmagnetic composition for a ceramic electronic component, a ceramic electronic component using the same, and a method for manufacturing the same. The nonmagnetic composition for a ceramic electronic component according to an embodiment of the present invention includes a compound represented by the formula ZnCuTiO 4 . According to one embodiment of the present invention, the inductance reduction rate at high current as well as the capacity change rate of the magnetic material after the application of the current according to the temperature change is insensitive to ensure stable operation characteristics of the ceramic electronic component.
priorityDate 2012-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004339031-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23954
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23978
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419557109
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID418354341
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14806
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID26042
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559192
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559214
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707770
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14829

Total number of triples: 37.