Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_56db81f6eb60da43b90fd720b484b743 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B11-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25C1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B25-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25C1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-44 |
filingDate |
2012-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_285b91d52945d5a3cffaddf08174e212 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00d6de8a8f8092a9898750fe9dae4e24 |
publicationDate |
2014-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101364520-B1 |
titleOfInvention |
Separation and Recovery of Useful Metals in Waste Lead-Free Solders Using Iron Chloride Solution |
abstract |
The present invention relates to a method for separating and recovering a useful metal from a waste lead-free solder using an iron chloride solution. The useful metal separation recovery method in the waste lead-free solder using the iron chloride solution according to the present invention includes a waste lead-free solder containing tin, copper and silver, and a solubility enhancer for enhancing the solubility of trivalent iron ions, tin and copper. Solvent in which solid silver and liquid tin ions and copper ions are dissolved through a leaching step of leaching tin and copper from the waste lead-free solder and precipitating silver from the lead-free solder, and solid-liquid separation after the leaching step. It comprises a solid-liquid separation step of separating each other and a selective recovery step of separating and recovering copper and silver from the solvent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015152457-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111705216-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101481366-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112708781-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112708781-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115637368-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115637368-A |
priorityDate |
2012-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |