http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101325307-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D2202-25 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D201-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D201-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C26-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 |
filingDate | 2011-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101325307-B1 |
titleOfInvention | Precoat aluminum plate and manufacturing method thereof |
abstract | As the precoat aluminum plate 10 which coated the hard film 2 of 0.2-7 micrometers in thickness on the surface of the aluminum plate 1, the hard film 2 consists of Si, F, C, O, N Regarding the total mass of the elements, the ratio of F is 1 to 25% and the ratio of Si is 1 to 50%, and a coating material containing Si and F is applied to the aluminum plate 1 to be 210 to 280 ° C. Characterized in that it is formed by baking. |
priorityDate | 2010-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.