http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101286786-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-322 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-40 |
filingDate | 2009-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101286786-B1 |
titleOfInvention | Preparation of absorbent article |
abstract | The manufacturing method of the water absorbent article by a 1st characteristic of this invention is a manufacturing method of the water absorbent article which has a base material and the film which becomes the urethane resin which has the water absorbency formed on the base material, The manufacturing method is application | coating of a coating liquid to the base material. The coating step has a step of supplying a coating liquid from a nozzle disposed above the substrate to the substrate surface of the substrate conveyed horizontally, wherein the coating liquid is polyisocyanate, polyol having ethylene oxide and hydrophobic It is set as having a solid content and a solvent to which a polyol is mixed, and it adjusts so that solid content concentration of a coating liquid may be 5-30 mass%, and a viscosity may be 1-3 mPa * s. |