http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101281969-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2555-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2555-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2555-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A30-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2555-64 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E01C7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L91-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E01C7-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 |
filingDate | 2011-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101281969-B1 |
titleOfInvention | Modifier composition for low-carbon, medium-temperature asphalt mixtures expressing a common grade of PB 64-22 or PP 70-22, and methods for preparing the asphalt mixture using the same |
abstract | The present invention relates to a modifier composition for a low carbon mesophilic type asphalt mixture expressing a common grade of PG 64-22 or PG 70-22, and a method for producing an asphalt mixture using the same, more specifically, 100 parts by weight of wax 4 In the modifier composition for low-carbon medium-temperature asphalt mixture, characterized in that the mixture is heated, melted, and mixed 4 ~ 30 parts by weight of the waste tire powder, and aggregate and asphalt, aggregate and filler material 94 It relates to a method for producing a low carbon mesophilic asphalt mixture, characterized in that ~ 96% by weight, asphalt and 4 to 6% by weight modifier are added and mixed in a plant mix. The low carbon mesophilic asphalt mixture according to the present invention enables the production of an effective mesophilic asphalt mixture (WMA) by a low carbon additive, and can reduce the heating energy required for the preparation of the mesophilic asphalt mixture, thereby reducing the amount of carbon dioxide which is the main culprit of global warming. It can significantly reduce the fuel consumption while minimizing the emission of other emulsifiers, and reduce the optimum mixing temperature and compaction temperature by about 15 ~ 25 ℃ compared to the prior art, resistance to high temperature plasticity change and low temperature cracking Common grades showing resistance express the performance of PG 64-22 or PG 70-22 and exhibit sufficient compaction. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9764984-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9969649-B2 |
priorityDate | 2011-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.