titleOfInvention | Copolyester having elastic recovery properties and manufacturing method thereof |
abstract | In the present invention, dimethyl terephthalate (Dimethyl Terephthalate (DMT) and dimethyl isophthalate (DMI) or terephthalic acid (Terephthalic acid (TPA) and isophthalic acid (Isophthalic Acid (IPA)) as an acid component (Diacid) ethylene glycol ( Ethylene glycol (EG), 1,4-butanediol (1,4-Butanediol: 1,4-BD), polytetramethyleneglycol (PTMG) is made of a diol component (copolymer) having an elastic recovery rate It is about. |