Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D7-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate |
2008-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2013-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101262435-B1 |
titleOfInvention |
Heat-shrinkable polyester film |
abstract |
The present invention relates to a heat-shrinkable polyester film, shrinkage by providing a heat-shrinkable polyester film having a rate of change in the shrinkage rate in the main shrinkage direction over time within 95 seconds at 95 ℃ 4.0 to 10.0% / sec By ensuring the uniformity of shrinkage in the process, the appearance quality is excellent, there is no occurrence of print distortion, and at the same time, there is an effect to reduce the production cost in the shrinkage process and improve productivity. |