http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101252110-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33f8096f7c6f74ac787c777aaf01104a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc97f70aef1120d77016fcac5764f032 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E30-30 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21C3-044 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21F9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21C19-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21F9-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21F9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21F9-30 |
filingDate | 2011-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b6a9d124d5159b69d176ea47806c280 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6119bc529cf37fe717a8721edb16860c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_06cdc9c9c18e8ab70b0e076d84a46f35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a786072272fbaa80219b4ecc7c9fd032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e6a49a69c6f1ed12d9287f55a46d85ce |
publicationDate | 2013-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101252110-B1 |
titleOfInvention | Method for producing porous sintered pellets for electrolytic reduction for recovery of metal nuclear fuel, which discontinuously conducts atmosphere sintering and reduction, and porous sintered pellets prepared accordingly |
abstract | The present invention relates to a method for producing a porous UO 2 sintered pellet for electrolytic reduction for the recovery of metal nuclear fuel, and to a porous UO 2 sintered pellet prepared according to the present invention, in detail oxidizing spent nuclear fuel containing uranium dioxide (UO 2 ) To form a powder comprising U 3 O 8 (step 1); Forming a powder by molding the powder formed in step 1 (step 2); Porous U 3 O 8 prepared in step 2 Sintering the molded body with an atmosphere gas at a temperature of 1200 to 1600 ° C. to produce UO 2 + x sintered pellets (step 3); And cooling the UO 2 + x sintered pellets prepared in step 3 to room temperature, and then reducing them to 1000 to 1400 ° C. in a reducing atmosphere to form UO 2 sintered pellets (step 4). Provided is a method for producing a porous UO 2 sintered pellet for feeding into the electrolytic reduction process. Accordingly, high quality porous UO 2 sintered pellets without cracks or the like can be manufactured. The prepared porous UO 2 sintered pellets can sufficiently remove volatile fission products and have an O / U ratio of 2.00, and include a large number of pores, which facilitate the penetration of electrolytes during the electrolytic reduction process, thereby increasing the rate of electrolytic reduction. have. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101711808-B1 |
priorityDate | 2011-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.