Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3225 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-5436 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3272 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2206-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2380-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2370-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2220-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C2360-46 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-119 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-4885 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-6455 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16C33-44 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C33-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C33-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C33-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C33-32 |
filingDate |
2010-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2013-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-101233869-B1 |
titleOfInvention |
Rolling bearing and its manufacturing method |
abstract |
To provide a rolling bearing having excellent acoustic properties and durability, which is preferable for applications requiring excellent anti-oiling effect, and low amount of lubricant or low torque of a bearing using a low viscosity lubricant. To this end, the present invention provides a rolling element comprising an alumina component and an yttria-zirconia component containing 1.5 to 5 mol% of a zirconia component or yttria in a mass ratio of an alumina component: a zirconia component or an yttria-zirconia component = 5 to It is made from the alumina-zirconia-based composite material which contains 50: 50-95. |