http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101219515-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-0573 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C33-0278 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C38-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C38-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-0578 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-023 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 |
filingDate | 2010-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101219515-B1 |
titleOfInvention | Method for producing R-Fee- 희 rare earth magnetic powder for bonded magnet, magnetic powder produced by this method and method for producing bonded magnet using the magnetic powder, bonded magnet produced thereby |
abstract | The present invention relates to a method for producing a R-FE-B rare earth magnetic powder for bonded magnets, a magnetic powder prepared by the same, and a method for producing a bonded magnet using the magnetic powder, and a bonded magnet manufactured by the same. Coarsely pulverizing the phosphorus rare earth sintered magnet product (step 1); A hydrogenation process step (step 2) of charging the pulverized product produced in the step 1 to a vacuum tube furnace and filling hydrogen and raising the temperature of the tube; A phase decomposition step (step 3) of further raising the temperature in the tube in the same hydrogen atmosphere as in step 2; Hydrogen discharge process step (step 4) for exhausting the hydrogen in the tube furnace of step 3; And a recombination process step (step 5) of evacuating the hydrogen pressure in the tube furnace after performing step 4, and a method of manufacturing magnetic powder with improved magnetic properties, thereby improving the magnetic properties. Provided are a magnetic powder prepared and a method for producing a bonded magnet using the magnetic powder, and a bond magnet manufactured thereby. Through the present invention, it is possible to manufacture a magnetic powder having a fine size and uniform composition to improve magnetic properties, and it is advantageous in terms of cost and environmental aspects by recycling waste scrap at low cost. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200009797-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102553034-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20230059534-A |
priorityDate | 2010-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 34.