http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101196530-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2459-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2333-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-042 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14688 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14811 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 |
filingDate | 2005-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2012-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101196530-B1 |
titleOfInvention | Injection molding simultaneous decorative sheet and decorative resin molded article |
abstract | The present invention comprises a base film and at least a decorative layer provided on the base film, wherein the elongation at break measured at 25 ° C. is 3 to 10% and the elongation at break measured at 120 ° C. is 200% or more. Provide a sheet. Laminated decorative sheets exhibit good agreement with the forming surface of the mold during the preforming process. When the sheet is laminated on and integrated with the resin molded body through injection molding, the wrinkles, bubbles, fractures, and the like appear less likely to occur. In addition, the decorative sheet can be easily trimmed.n n n n Decorative sheet, injection molding, molded products, elongation at break, preforming |
priorityDate | 2004-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |