abstract |
The invention relates to (a) a unit derived from about 5% to about 35% by weight of an alpha-olefin, and a propylene-based elastomer characterized by a heat of fusion as measured by DSC, of less than 80 J / g, (b) about A propylene-based thermoplastic polymer characterized by an MFR of 3 to about 300 dg / min (ASTM D-1238, 2.16 kg, at 230 ° C.), and a heat of fusion greater than 80 J / g as measured by DSC, and (c) (i ) High-MFR thermoplastic resin having an MFR greater than 400 dg / min (ASTM D-1238, 2.16 kg, at 230 ° C.), (ii) hydrocarbon resin, (iii) polyolefin wax, (iv) functionalized hydrocarbon resin, A nonwoven fiber made from a composition comprising (v) a functionalized polyolefin, and (vi) a feel modifier selected from the group consisting of two or more combinations of the foregoing feel modifiers, and (d) optionally a slip aid. |