http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101008201-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-127 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-125 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C8-02 |
filingDate | 2008-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2011-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101008201-B1 |
titleOfInvention | Frit composition for sealing flat panel display panels |
abstract | The present invention relates to a frit composition for sealing a flat panel display panel, more specifically, Bi 2 O 3 (A) 30 to 45 mol% (mole%), ZnO (B) 13 to 35 mol%, B 2 O 3 ( C) 15 to 35 mol%, Al 2 O 3 (D) 0.1 to 3 mol%, R 2 O (E) 0 to 5 mol% (The R 2 O is Li 2 O, Na 2 O, K 2 O and At least one selected from the group consisting of Cs 2 O), R'O (F) 0 to 5 mol% (The R'O is at least one selected from the group consisting of MgO, BaO, CaO and SrO), The mother glass 60 to 95 having A ≧ (B + C) / 2 and satisfying E + F ≧ 0.1 and having a Tg (glass transition temperature) of 400 ° C. or lower and a thermal expansion coefficient of 70 to 105 × 10 −7 / ° C. The present invention relates to a sealing frit composition comprising a weight% and the remaining low-expansion ceramic filler, wherein the frit composition for sealing a flat panel display panel of the present invention does not contain a lead component and thus does not have a problem of environmental pollution. Soften to the extent possible Low point and glass transition temperature, excellent fluidity, no problem of crystallization and the like, excellent reliability and durability after encapsulation, and reduced energy and time in the encapsulation process, resulting in improved flat panel display panel productivity and reduced manufacturing cost.n n n n Lead-free, frit, flat panel display panels, sealed, low temperature fired |
priorityDate | 2008-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |