http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101002714-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A41D2500-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2101-38 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A41D19-015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A41D19-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A41D19-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A41D19-00 |
filingDate | 2008-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2010-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2010-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-101002714-B1 |
titleOfInvention | Water-based polyurethane coating composition and manufacturing method of water-based polyurethane coated gloves with excellent moisture permeability and wear resistance |
abstract | The present invention relates to a method for preparing a water-dispersible polyurethane with an anionic group such as a carboxyl group or a sulfonate group or a cationic group such as a tertiary amine in the main chain, and wet-coagulating it to prepare an aqueous polyurethane moisture-permeable coated glove. After impregnating and coating the endothelial glove woven with various yarns (nylon, polyester, polyethylene, kevlar and cotton, etc.), a mixture of water repellent, dispersant, antifoaming agent, colorant, viscosity control agent and other additives , Coagulate with a coagulation solution (coagulation solution consisting of an aqueous solution of an acid, an aqueous solution of a salt, a base solution or a mixture of two or more thereof) to form micropores to impart air permeability, and the aqueous polyurethane is coated through a washing process, drying, and a crosslinking process. Method of manufacturing environmentally friendly breathable gloves.n n n The glove manufactured by the manufacturing method of the present invention has a better wear resistance due to the stronger film strength of the surface than conventional oil-based polyurethane wet products, and has a low slip when the gloves are worn by penetrating the resin to the back of the endothelial, which is excellent in workability and uniformity. It has the characteristics of breathability, soft fit and eco-friendly coating gloves due to micropores.n n n The manufacturing method of the present invention can use the existing oil-based wet process as it is, do not use any organic solvents such as DMF (Dimethyl formamide) is environmentally friendly, excellent coating molding manufacturing to improve glove productivity by excellent de-molding It is a way.n n n n Water-based polyurethane, coated gloves, moisture permeability, wear resistance |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101936882-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102301468-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102349984-B1 |
priorityDate | 2008-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 212.