http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100926714-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4854 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate | 2003-04-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100926714-B1 |
titleOfInvention | Resin composition for optical fiber coating and coated optical fiber and optical fiber unit using the same |
abstract | Resin composition for optical fiber coating containing a radically polymerizable oligomer (A) and a radically polymerizable monomer (B), wherein said (A) is a compound of following (1)-(3): (1) Number average molecular weights 50- A radically polymerizable oligomer having a number average molecular weight of 600 to 1,600 formed by reacting an aliphatic polyol compound of 600, (2) a polyisocyanate compound having a cyclic structure, and (3) a compound having a hydroxyl group and a radical polymerizable unsaturated group in the same molecule ( A1) and the following compounds (4) to (6): (4) an aliphatic polyol compound having a number average molecular weight of 800 to 10,000, (5) a polyisocyanate compound, and (6) a compound having a hydroxyl group and a radical polymerizable unsaturated group A radically polymerizable oligomer (A2) formed by reacting the same, and the mass ratio (A1) / (A2) of the above (A1) and (A2) is 20/80 to 80/20, and in the resin composition for coating the optical fiber Urethane bond concentration is 1.85 to 3.0 Resin composition for optical fiber coating which is 0 mol / kg. |
priorityDate | 2002-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 121.