http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100885218-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L29-015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A23L7-1963 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23L7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A23L7-196 |
filingDate | 2006-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100885218-B1 |
titleOfInvention | Rice processing method |
abstract | The present invention relates to a processing method of rice, and more particularly, a rare earth-based natural mineral powder is coated on brown rice, in which rice is first coated, and stored for a long time by anion emanation and mineral adsorption of minerals. The present invention relates to a rice rice coated with rice bran oil to improve the taste of rice and provide various nutrients without deterioration and removal of residual pesticides.n n n The present invention described above, the step of collecting illite, chlorite, respectively, which exists as a natural mineral in a natural state; Crushing the collected minerals into coarse particles to remove impurities, and then drying the water into a drying furnace to completely dry the moisture contained in the minerals while applying heat of 500 to 700 ° C .; Pulverizing the dried minerals finely to form a fine powder of mineral powder by sieving each of them with a sieve maintaining a particle size of 200 mesh or more; 94 to 96% by weight of rice hulled from rice, 3 to 4% by weight of illite powder, and 1 to 2% by weight of chlorite powder are added to the mixer and mixed evenly. Evenly coating the aelite and the chromite powder; Storing the brown rice coated with the illite and the chromite powder for at least 24 hours; Milling brown rice to maintain 92% of white rice and processing white rice; Rice bran oil and rice extracted from rice bran and rice flakes are added to the mixer so that the amount of rice is 1: 400% by weight so that the rice bran oil is evenly coated on the surface of the rice; Rice can be achieved by a processing method of rice, characterized in that the step consisting of vacuum packaging the rice coated with oil.n n n n Brown rice, illite, chromite, anion, milling, white rice, brown rice oil |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160073808-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101430311-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160081112-A |
priorityDate | 2006-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.