http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100821679-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f997f1a2868e0854ad284e7b28da8702 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B44C1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B21D53-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B44C5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C65-2015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A47G1-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47G1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B21D53-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B44C1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B44C5-00 |
filingDate | 2007-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7430d45f0d3b6771226c256f35ff5b2 |
publicationDate | 2008-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100821679-B1 |
titleOfInvention | Method for manufacturing decorative mirror using laser-processed steel sheet and decorative mirror manufactured by the method |
abstract | The present invention relates to a method of manufacturing a decorative mirror using a laser-processed iron plate and a decorative mirror manufactured by the method. More specifically, the present invention can not only play a sufficient role as an interior accessory but also pursue a beautiful exterior. The present invention relates to a method of manufacturing a decorative mirror using a laser-processed steel sheet and a decorative mirror manufactured by the method, which can enhance the value as a high-value-added product having a natural look and splendor.n n n To this end, the present invention comprises the steps of: (a) designing the shape of the decorative portion to be formed in the decorative mirror; (b) processing the iron plate prepared to conform to the shape of the design while providing at least one hole in the plate surface to prepare a laser processed iron plate; (c) forming a putty layer on the surface of the laser processed iron sheet; (d) forming a decorative thin film layer on the surface of the putty layer; (e) attaching the finished iron plate unit of the intermediate stage completed to step (d) to the surface of the mirror; And (f) attaching a decorative ball to the hole. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101987557-A |
priorityDate | 2007-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.