http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100813797-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8d6fd91d4d473aac9e5574eabb479e5b |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-00 |
filingDate | 2006-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccab9473f6b98fb7b6369e2cdef0ad2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_186a338990d88d2d5f23b50e283a3128 |
publicationDate | 2008-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100813797-B1 |
titleOfInvention | Hazardous Substance Reduction Catalyst, its Manufacturing Method and Environmental Performance Improvement Using It |
abstract | The present invention relates to a catalyst for reducing harmful substances, a method of manufacturing the same, and a building material using the same, and an object thereof is to add a hazardous substance reducing catalyst that can be added to a building material such as an adhesive or a paint to reduce harmful substances emitted from the building material. It is to provide a manufacturing method.n n n In the present invention, a stabilized divalent metal compound such as Fe (II), Cu (II), Zn (II) or the like is slowly added with ultrapure distilled water at a temperature of 40 ° C. to 50 ° C. and atmospheric pressure, and a chelating agent solution is added to the solution. Is added at a temperature of 100 ℃ to 110 ℃, it is stirred for about 5 to 10 hours to form a first mixture, and the mixture is mixed with a carrier, a thickener, and a polymer resin to the first mixture harmful substances A reduction catalyst is produced, and the harmful substance reduction catalyst is added to 5 to 15% by weight of building materials such as adhesive or paint. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101717620-B1 |
priorityDate | 2006-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.