classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-4922 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-009 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B41-64 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-02 |
filingDate | 2005-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100809809-B1 |
titleOfInvention | Manufacturing method of surface penetration reinforcement for preventing concrete deterioration |
abstract | The present invention relates to a method for preparing a surface penetration reinforcing agent for preventing concrete deterioration, and more specifically, to prepare a surface penetration reinforcing agent by synthesizing a monomer having an OH functional group and an inorganic material of a silicate series containing an ethoxy or methoxy group. By applying this to the surface of the concrete structure using a spray gun or a brush, the penetrating surface penetration reinforcing agent is hydrolyzed by the water present in the concrete to form silica (SiO 2 ) of several nanometers in size, and then a sol-gel As the gelation proceeds through the process, the reactant with the concrete hydrate densely fills the voids in the concrete, so the surface penetration for preventing concrete deterioration has the effect of increasing the strength of the concrete structure, inhibiting the penetration of deteriorated materials, and preventing waterproofing and neutralization. It relates to a method for producing a reinforcing agent.n n n n Concrete, surface penetration reinforcement, deterioration prevention, concrete reinforcement, silicate, monomer |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100863978-B1 |
priorityDate | 2005-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |