http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100805517-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J2211-42 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7734 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J9-227 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-22 |
filingDate | 2004-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100805517-B1 |
titleOfInvention | Method for manufacturing plasma display device and phosphor |
abstract | A phosphor in which the mother crystal is composed of an oxide, which is a method of producing a phosphor having less oxygen defects in the phosphor, and a plasma display device using the same. After the step of weighing, mixing, and filling the powder of the phosphor, the step of firing at least one time in a reducing atmosphere, and the step of firing in an oxidizing atmosphere after the treatment step in the last reducing atmosphere, and further in a processing step in an oxidizing atmosphere The firing temperature of is set to 600 ° C or higher and 1000 ° C or lower. |