http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100793460-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23Q2703-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23Q2703-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23Q3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23Q3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23Q3-084 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23Q3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23Q3-00 |
filingDate | 2006-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2008-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-01-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100793460-B1 |
titleOfInvention | Melting / Coagulation Fixtures for Machining and Machining Methods |
abstract | This invention improves the adhesive strength of a workpiece | work, and also simplifies the washing | cleaning process after machining of the melting / coagulation fixative for machining which uses shellac resin. According to the present invention, a powdery rosin of 10 to 95% by weight is mixed with an unheated powdery shellac resin to prepare a melting / coagulating fixative for machining. |
priorityDate | 2005-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |