http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100788259-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-47 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-06 |
filingDate | 2006-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100788259-B1 |
titleOfInvention | Manufacturing Method of Positive Tip Sea Plate Using Antistatic Alignment Film |
abstract | The present invention provides a method for producing a + C-plate using an antistatic alignment film, comprising: (a) an alignment film comprising an alignment film coating composition comprising an alignment film resin, a curing agent, an antistatic agent, a photopolymerization initiator, and a leveling agent in a solvent; 100% by weight of the coating solution, i) 15% by weight to 55% by weight of the alignment film resin ii) 0.1% by weight to 10% by weight of the curing agent i) 1.5% by weight to 5.5% by weight of the antistatic agent 1% by weight to 6% by weight ⅴ) The leveling agent is coated with an alignment film coating solution mixed at 0.1% by weight to 3% by weight according to the inline coating method on a transparent support, and then dried and UV cured to form an alignment film. Forming step; (b) a rubbing step of rubbing the alignment film formed in the step in the longitudinal direction of the transparent support; And (c) coating a liquid crystal coating solution containing 15 wt% to 60 wt% of the nematic liquid crystal mixed on the rubbed alignment layer by an in-line coating method, and drying and UV curing to form a liquid crystal layer. It is carried out including. |
priorityDate | 2006-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |