http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100695546-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 2001-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100695546-B1 |
titleOfInvention | Low-fogging Thermoplastic Elastomer Compositions and Methods of Making and Uses of the Compositions |
abstract | The present invention is 10 to 90 parts by weight of crystalline polyolefin (a), 90 to 10 parts by weight of olefin copolymer rubber (b) (the total amount of components (a) and (b) is 100 parts by weight), 200 ° C, Fully or partially crosslinked olefinic thermoplastic elastomer composition having 3 to 100 parts by weight of paraffinic mineral oil softener (c) having an evaporation loss of 0.4% by weight or less at atmospheric pressure and 1 hour and having a kinematic viscosity (40 ° C.) of 50 to 250 cSt. ; 40 to 85 parts by weight of the ethylene copolymer rubber (A), 60 to 15 parts by weight of the olefinic resin (B) and 45 parts by weight or less of the softener (C) [the total amount of the components (A), (B) and (C) 100 parts by weight] of the mixture containing the glass sheet, which is obtained by dynamically heat treatment in the presence of a crosslinking agent and subjected to fogging test under conditions of 100 ° C. and 3 hours in accordance with DIN 75201 A method using 10 g of pellets. An olefinic thermoplastic elastomer composition having a gloss value of 80% or more and a haze value of 10% or less; And to methods and uses for the preparation of such compositions.n n n Low Foaming Thermoplastic Elastomer Composition, Mineral Oil Softener |