http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100687943-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F297-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-01 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D153-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 2005-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100687943-B1 |
titleOfInvention | Hydrogenated styrenic block copolymer composition with improved high temperature extruded properties |
abstract | A) Hydrogenated styrene having a dendritic endblock of at least two polymerized monovinyl arenes and an elastomeric intermediate block composed of polymerized and subsequently hydrogenated conjugated dienes or dienes, which can be used for external molding on a polar substrate. System block copolymers 100 pbw, b) 25 to 60 pbw functionalized polyolefin and optionally c) 0 to 100 pbw plasticizer, d) one or more fillers and 0 to 200 pbw filler inactivating agent and e) 0 to 2 pbw antioxidant and f) a hydrogenated styrenic block copolymer composition containing 0-100 pbw of an engineering polar thermoplastic, wherein component (a) is a hydrogenated linear styrene-based block air having an apparent molecular weight in the range of 200,000 to 500,000. Coalesced or hydrogenated radial styrenic block copolymers having an apparent molecular weight ranging from n × 100,000 to n × 250,000, where n is the polymer fraction Component (a) has a hydrogenated 1,2-polymerized conjugated diene content (vinyl content) of more than 40% and a poly (monovinyl arene) content in the range of 20 to 50%, ) Is an acid, anhydrous or ester functionalized polyolefin having a grafting rate of 0.5 to 5 wt% and a melt flow rate of at least 20 g per 10 minutes (MFR, ASTM D 1238-95, condition L).n n n Hydrogenated styrenic block copolymers, external molding, polyamides, melt flow rates, polyolefins |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100810564-B1 |
priorityDate | 2004-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 60.