http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100676118-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2205-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2290-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6688 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-72 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate | 1999-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100676118-B1 |
titleOfInvention | Semi-rigid polyurethane foam |
abstract | To provide a semi-rigid polyurethane foam that is difficult to produce fogging even at high temperature, and can be suitably used for automobile interior materials.n n n The haze value in the fogging test is 70% or more of strength retention at high temperature standing (120 ° C. × 24 hours standing), which is obtained by mixing and stirring a polyol mixture containing polyol, water, and a catalyst and polyisocyanate. A semi-hard polyurethane foam having two or less. |
priorityDate | 1999-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |