http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100654089-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6aed259b0a96df1f6a877f0b2f8586d4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A45D2024-002 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A46B15-0024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F8-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A45D24-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A45D24-00 |
filingDate | 2005-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2006-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c342f34566d5b8d9ba9831122d238204 |
publicationDate | 2006-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100654089-B1 |
titleOfInvention | Method for manufacturing hairbrush comb |
abstract | The present invention relates to a method for manufacturing a hairbrush comb, more specifically, a hairbrush comb contains a tourmaline powder that emits a large amount of anions and far infrared rays and a nanosilver solution having an antimicrobial action to promote blood circulation of the scalp. It relates to an invention to keep the scalp and hair healthy.n n n Features of the present invention described above, preparing a nano-silver solution of the colloid on the polyvinyl pyrrolidone (PolyVinylPyrrolidone) conjugated to the nano-silver particles of the metal prepared by ion reduction of silver nitrate (AgNO 3); Preparing fine powder to generate anion by collecting tourmaline, which is a mineral, and finely pulverizing it, and then filtering it with a sieve having a particle size of 500 mesh or more; A drying step of spraying 80 to 100 ° C. hot air to the nylon raw chips in a drying chamber for 3 to 4 hours to evaporate the solvent component and water contained in the raw chip; Mixing the white titanium powder evenly so as to be 0.2 to 0.4% by weight of the raw material chip so that the titanium powder is evenly coated on the surface of the raw material chip; 95-97% by weight of a nylon powder chip coated with titanium powder, 2-4% by weight tourmaline powder, and 0.8-1.2% by weight nanosilver solution; Putting a nylon raw material chip mixed with tourmaline powder and a nanosilver solution into an extruder, and then heating and melting it, and extruding the molten chip raw material to form a round rod; The long molded nylon molding can be achieved by a method of manufacturing a hair brush comb, characterized in that the step of completing a comb by cutting to a predetermined length after cooling to a low temperature. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101698496-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101410787-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101994364-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160131630-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2233029-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170005949-A |
priorityDate | 2005-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.