http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100633177-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-329 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-309 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-387 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2227 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-02 |
filingDate | 2005-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100633177-B1 |
titleOfInvention | Room temperature drying inorganic coating composition using pH control and its manufacturing method and use |
abstract | The present invention relates to a room temperature dried inorganic coating composition using pH control, a method for producing the same, and a use thereof, and an object thereof is an inorganic coating composition obtained by hydrolyzing alkoxysilane, at least one selected from an alkali solution or a buffer solution. By adding and maintaining the pH of the paint to increase the pot life, shorten the curing time, and drying at room temperature, at room temperature drying inorganic coating composition that can be applied to anyone without special restrictions and its manufacturing method and uses To provide.n n n The present invention is 1 to 40% by weight of the organo alkoxysilane represented by the general formula R n Si (OR ') 4-n ; 0.5 to 20% by weight of a colloidal oxide containing water or an organic solvent as a dispersion medium in terms of solid content; 0.1-70% by weight of lower aliphatic alcohol; 0.1-3 wt.% Organic / inorganic acid; 0.01-20 wt% of inorganic filler; 0.01-40 weight% of inorganic pigments; Alkaline solution, buffer solution consists of 0.1 to 5% by weight of a single or mixed pH stabilizer. Wherein R is an alkyl group having 1 to 6 carbon atoms, R 'is an alkyl group having 1 to 5 carbon atoms or an acyl group having 1 to 4 carbon atoms.n n n n Inorganic paint, room temperature drying, pH control, buffer solution, alkaline solution |
priorityDate | 2005-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 119.