http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100547955-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-383 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B22-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B18-0445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B38-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-16 |
filingDate | 2003-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2006-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2006-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100547955-B1 |
titleOfInvention | Non-combustible, heat insulation, heat insulation, absorption. Construction method of foamed concrete mortar with sound insulation |
abstract | The present invention is 30 to 70% by weight of hot phosphate gypsum and / or 30 to 70% by weight of the dried granite stone powder and / or dried at a temperature of 150 ℃ to 800 ℃ to stabilize the pollutants impregnated with moisture removal 30 to 70% by weight of dried waste limestone as the main material, 20 to 40% by weight of cement, yellow or kaolin, feldspar 2 to 10% by weight, foaming agent (alumina powder, zinc powder) 0.01 to 0.5% by weight, 2 to 5% by weight of foaming catalyst (quick lime and carbonate), 0.01 to 5% by weight of anti-separation stabilizer (methylcellulose, wood flour or rice husk powder), 0.5 to 3% by weight of concrete strength reinforcement, 3 to 15% by weight of tensile strength reinforcement Dry mixed and then mixed and agitated 50 ~ 85% water of the mixed mortar weight at the construction site to maintain a uniform turbidity, 20 minutes to 50 minutes after the complete foam group is formed non-flammable, heat insulation, Insulation, absorption. It is to provide a construction method of foamed concrete mortar having a sound insulation function.n n n n nIncombustible, insulated, absorbent. Sound insulation, phosphate gypsum, ocher, carbonate, |