http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100538507-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2969 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H2701-313 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2929 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65H55-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65H55-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14 |
filingDate | 2002-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100538507-B1 |
titleOfInvention | Polyester Composite Fiber Pirn and Production Method Therefor |
abstract | The present invention is composed of a single yarn in which two kinds of polyester components are joined in a side by-side type or an eccentric ultracentrifugal form, and at least one of the polyester components constituting the single yarn is 90 mol% or more in the repetition of trimethylene terephthalate. The composite fiber which is the polytrimethylene terephthalate which consists of a unit is wound in the shape of a fern, The winding amount of this composite fiber fern is 1 kg or more, The taper winding angle is 15-21 degrees, The winding hardness of a cylindrical part is 75-92, It provides a polyester-based composite fiber fern, characterized in that the heat shrinkage stress expression start temperature of the composite fiber is 50 to 80 ℃. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101228760-B1 |
priorityDate | 2001-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.