http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100526929-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31703 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31678 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2439-70 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-085 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 1999-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100526929-B1 |
titleOfInvention | Laminated film |
abstract | The present invention has a density (d; measured according to ASTM D 1505) prepared using a metallocene olefin polymerization catalyst of 0.895 to 0.930 g / cm 3 , a melt flow rate (temperature 190 ° C. according to ASTM D 1238, and a load of 2.16 kg). Is a laminate film obtained by extrusion lamination of a linear low density polyethylene layer having a thickness of 0.1 to 100 g / 10 minutes on one side of an aluminum layer (A), wherein the oxygen concentration of the linear low density polyethylene itself is 1.0 at the surface of the linear low density polyethylene layer. A laminated film which is -1.4 atomic%. Excellent balance of aluminum adhesive strength and heat sealability of linear low density polyethylene and can be provided at low cost. In addition, the laminated film can be provided at a low cost by laminating a linear low density polyethylene layer, an aluminum layer and a base layer by an extrusion lamination method in order. This laminated film is suitable for packaging materials for dry food, for example. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101504434-B1 |
priorityDate | 1998-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 130.