http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100526246-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2023-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2023-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2029-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2509-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2067-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S425-048 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C35-0805 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-10 |
filingDate | 2003-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100526246-B1 |
titleOfInvention | Method of producing a ceramic sheet |
abstract | The present invention relates to a method for manufacturing a ceramic sheet, comprising: mixing a polymer material and a ceramic powder, extruding the mixed material into a base film having a first thickness, and each of a plurality of substrates on at least both ends of the base film. Mounting a grip, scanning a high frequency of at least about 1 MHz or more into the base film to heat the base film to a stretchable temperature, and scanning the high frequency to maintain the heated temperature; It provides a ceramic sheet manufacturing method comprising the step of forming by using the two grips to form a ceramic sheet of a second thickness less than the first thickness.n n n The ceramic sheet manufacturing method using the ultra-high frequency according to the present invention can not only damage the base film by the selectivity of the heating portion, but also can be quickly heated to a stretchable temperature, thereby reducing the overall manufacturing process time It is expected. |
priorityDate | 2003-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6585 http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415823930 |
Total number of triples: 24.