http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100525780-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-485 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 |
filingDate | 2003-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100525780-B1 |
titleOfInvention | A Cathode Material for Secondary Batteries with Non-Aqueous Electrolyte and a Process for preparing the Cathode Material |
abstract | The present invention relates to a positive electrode active material for a non-aqueous electrolyte secondary battery, and more particularly, LiNi x M a M ' b M " c O 2 (In the above, M, M' are each independently a transition metal element, M" is It is a non-transition metal, At this time, it relates to the positive electrode active material for secondary batteries of a non-aqueous electrolyte containing the lithium nickel complex oxide and Pb compound represented by x + a + b + c = 1, and 0 <a + b + c ≦ 0.5.n n n When the positive electrode active material according to the present invention is applied to a secondary battery of a non-aqueous electrolyte, the high temperature thermal stability is high without sacrificing capacity, and as a result, it is possible to suppress the reactivity with the electrolyte solution, thus leaving the battery at a high temperature. When the battery swelling is significantly reduced. In addition, the cathode active material according to the present invention may be manufactured by various methods. |
priorityDate | 2003-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |