http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100515587-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-53 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 |
filingDate | 2002-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100515587-B1 |
titleOfInvention | Acrylonitrile-butadiene-styrene graft copolymer composition and method for preparing thereof |
abstract | FIELD OF THE INVENTION The present invention relates to acrylonitrile-butadiene-styrene graft copolymers and methods for preparing the same, in particular, inner layers and glass transition temperatures (Tg) having a glass transition temperature (Tg) of at least 0 ° C. and an average particle diameter of up to 2000 kPa. Is a multi-layered rubber polymer having an outer layer having a maximum particle size of -20 ° C. and an average particle diameter of 2500 to 5000 kPa, a large diameter rubber polymer having an average particle diameter of 2500 to 5000 kPa, a gel content of 60 to 95% and an swelling index of 18 to 40. Graft copolymerization of an aromatic vinyl compound and a vinyl cyan compound into the mixed rubber polymer mixed to provide acrylonitrile-butadiene-styrene graph with excellent impact resistance, tensile property, and gloss, and particularly excellent coloring and low temperature impact resistance. The present invention relates to a copolymer and a method for producing the same. |