http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100515404-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-00 |
filingDate | 2002-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100515404-B1 |
titleOfInvention | A method for the preparation of bone filler with rugged surface |
abstract | The present invention relates to a method for preparing a surface irregularity bone filler by adding a) a mixture of a flammable liquid temporary agent and a surfactant to a slurry of a) a mixture of bioactive ceramics and a water-soluble organic component binder, and more specifically, Preparing a slurry in which bioactive ceramics and a water-soluble organic component binder are mixed; Preparing a solution in which a flammable liquid temporary agent and a surfactant were mixed, and mixing them with each other; Stirring the solution sufficiently to form a homogenized slurry; Molding it; dry; Degreasing; Sintering; Through the continuous process of grinding and sieving to prepare a surface irregularity bone filler. The bone filler of the present invention can easily control the pore size and porosity of the desired conditions, the mechanical properties are improved and economical and reproducibility is excellent, it is suitable for mass production. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101094168-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101077095-B1 |
priorityDate | 2002-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.