abstract |
On a surface of at least one side of the base paper, a recording layer composed mainly of synthetic silica and an aqueous binder is formed at a solid content of 0.5 to 4.0 g / m 2 per surface. A recording paper made of a recording paper, wherein the critical surface tension γ c of the surface of the recording layer is 32 ≦ γ c ≦ 42 dynes / cm, or the contact angle of the surface of the recording layer measured using water is 100 ° to 120 °. Or the critical surface tension (γ c) of the surface of the recording layer is 32 ≦ γ c ≦ 42 dyne / cm, and the contact angle measured using water is 100 ° to 120 °. |