Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-0133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31518 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31511 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-0212 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-05 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-323 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-22 |
filingDate |
2000-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2003-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2003-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-100402154-B1 |
titleOfInvention |
Anisotropically conductive paste |
abstract |
The ion conductivity of the aqueous solution obtained by mixing the conductive paste and pure water is 1 mS / m or less; The viscosity at 80-100 ° C. of the B staging composition is 50-10000 Pa · s; The linear expansion coefficient at 0-100 degreeC of the hardened | cured material of an anisotropic conductive paste is 10x10 < -5> mm / mm / degrees C or less, heat distortion temperature Tg is 100 degreeC or more, water absorption is 2 mass% or less, and specific resistance is 1x. It is 10 9 Pa.cm or more, The anisotropic conductive paste is provided. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101279980-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101385032-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101553436-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101434688-B1 |
priorityDate |
1999-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |