http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100386192-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2321-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-28 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L17-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C- http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C- http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J- http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B- http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L- |
filingDate | 1995-06-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2003-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2003-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100386192-B1 |
titleOfInvention | Improvements in and relating to the reclaiming of elastomeric materials |
abstract | The present invention provides a sulfur-treated process consisting of kneading the rubber material at temperatures below 50 ° C. using a novel chemical mixture capable of initiating proton exchange in a controlled manner to open or degrade the vulcanized network of rubber material. It relates to reusing used rubber materials. The novel chemical mixtures are made of one or more compounds that can act as rubber promoters and one or more active agents capable of initiating proton transitions at temperatures of up to 70 ° C., thereby opening or breaking down the vulcanized network of sulfur-treated rubber materials. Thereby providing a regenerated rubber material that can be sulfur-treated.n n n Preferred mixtures consist of a molar ratio of zinc salt of dimethyldithiocarbamate and 2-mercaptobenzothiazole in the range of 1: 1 to 1:12, wherein the two materials are preferably dispersed in diols and stearic acid Activated by zinc oxide and sulfur. This mixture, when mixed with the vulcanized rubber pulverization in a rolling mill at a concentration of 6 parts by weight of binder per 100 parts by weight of the rubber pulverization, effectively breaks down the vulcanized network and allows the compound to be shaped and vulcanized. The resulting recycled rubber compound exhibits satisfactory levels of physical and mechanical properties. Such compounds can be used directly in tires and mixtures with molded or unused compounds in the related art. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180055536-A |
priorityDate | 1994-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 84.