http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100384563-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aafe0172ffd94d3486c518b0709bb2b3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F236-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-04 |
filingDate | 1997-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2003-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_56a874025fe1537a34294b5874dd819a |
publicationDate | 2003-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100384563-B1 |
titleOfInvention | Rubber modified thermoplastic composite material and manufacturing method |
abstract | The present invention is 5 to 20 parts by weight of a rubber polymer; 80 to 95 parts by weight of one or two or more monomer mixtures selected from the group consisting of aromatic vinyl compounds, vinyl cyanide compounds, unsaturated carboxylic acids, and ester compounds; Inorganic additives include 0.01 to 50 parts by weight of organically treated clay minerals; 0.2 to 0.3 parts by weight of the initiator; And 0.04 to 0.06 parts by weight of a molecular weight regulator are mixed in the first reactor, the solution is polymerized under high shear agitation to convert the phase of the rubber component into dispersed particles, and then the polymerization is continued in the second reactor in the range of 1 to 5 microns. Rubber polymer particles having a diameter are formed to form a basic form of rubber-modified thermoplastic resin dispersed in the matrix thermoplastic resin, wherein the clay mineral is nano-size simultaneously in the rubber polymer particles or in the matrix resin or in the rubber particles and the matrix resin simultaneously. It is a rubber-modified thermoplastic composite having excellent mechanical properties and thermal stability without deterioration of impact resistance having a structure dispersed in (nano-size) size. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100450640-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100450639-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20040042353-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100814553-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030056335-A |
priorityDate | 1997-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 111.