http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100309315-B1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3778e28a1c12f9c8e697759a4b573ff4
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-52
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-363
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B3-12
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-26
filingDate 1999-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2001-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65283152ea194bca0dc18ba15a0918ea
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98852c87da044620111ae3373141f35d
publicationDate 2001-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber KR-100309315-B1
titleOfInvention The method for preparing for soundprofing and dustprofing compounds
abstract The present invention relates to a self-adhesive rubber-asphalt-based soundproofing and a dustproof material, and, in detail, relates to a self-adhesive rubber-asphalt-based soundproofing, a dustproof material and a manufacturing method thereof for reducing noise and vibration generated in a vehicle or an industrial device.n n n 2-10% by weight of synthetic rubber, 50-65% by weight of ferrite (magnetite powder), 10-20% by weight of calcium carbonate, 15-25% by weight of blown asphalt, 5-15% by weight of mica, fiber The composition was weighed at a composition ratio of 2 to 5% by weight, 1 to 2% by weight of vulcanizing aid, and 0.1 to 0.5% by weight of curing agent, and then the mixture was sufficiently stirred within 5 minutes in a range of 70 to 120 ° C in a mixer. Then, the sheet is formed into a thickness of 1 to 6 mm using a calendar roll (temperature of 65 to 100 ° C.), and then the manufactured sheet is moved by a conveyor and sent to an embossing process so that the temperature is embossed at about 50 to 80 ° C. The part of the embossed pattern that is continuously connected to each other has a unique shape (see FIG. 2) that does not coincide with each other. The sheet passed through the embossing process is cooled by a continuous conveyor while the temperature is 50 ° C. or lower. Magnets in sheets continuously as a magnetizer of drum type I light and magnetized to have a magnetic force less than 300 gauss, through an adhesive applying step of the calender type by the sheet passing through the magnetization process is continued conveyor operation temperature of the adhesive applicator is about 150~180 ℃ range. After applying the hot melt, the sheet passing the process is passed through the shape punching process, and then packaged in a conventional manner, the vehicle and industrial self-adhesive rubber-asphalt-based sound-proof dust-proof material and a manufacturing method thereof .
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100471710-B1
priorityDate 1999-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19980025322-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19980033587-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-19980027899-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-S6114256-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419525871
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14789
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10112
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID453467280

Total number of triples: 27.