http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100290707-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-098 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-098 |
filingDate | 1998-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2001-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2001-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100290707-B1 |
titleOfInvention | Manufacturing method of polyether high elastic elastic yarn |
abstract | The present invention extends 1.01 to 2.01 times between the first high roller and the second high roller between the first high roller and the second high roller when melt spinning the polyether polyester having PBT-based polyester as the hard segment and PTMG as the soft segment. In addition, it is a manufacturing method of high elastic elastic yarn having an elastic recovery rate of about 88% even under high elongation of 200%. |