http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100275808-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 1999-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2000-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_40f95479608b44ddb34e6ad28148b153 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_27ef6c95aab2756d9d6e7c038257b2cb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_335eb584280c342f5a05fa2d2bf78d65 |
publicationDate | 2000-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100275808-B1 |
titleOfInvention | Styrene resin and resin composition comprising the same |
abstract | The present invention relates to a styrene resin excellent in moldability and physical properties and suitable for recycling, and to a composition of the styrene resin and a thermoplastic polycarbonate resin. More specifically, the present invention relates to a styrene resin having excellent moldability, not easily subjected to thermal degradation, and having improved heat resistance and impact strength, and a composition of the styrene resin and a thermoplastic polycarbonate resin.n n n Styrene resin according to the present invention 50 to 90% by weight of the continuous phase component (S) consisting of a copolymer such as styrene monomer, unsaturated nitrile monomer; And 10 to 50% by weight of the dispersed phase component consisting of a rubbery polymer component containing the monomer and grafted with the copolymer, wherein the triple continuous chain unit AAA is the continuous phase component (S). ) Is not detected from the unsaturated nitrile monomer unit (A); The amount of double continuous chain units AA is 3% or less based on the total units (A) detected; The reduced viscosity (ηsp / c) of the continuous phase component (S) is 0.2 to 0.85 dl / g; Specific impurities are not contained in an amount exceeding a predetermined amount. |