http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100260375-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-06 |
filingDate | 1997-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2000-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f9fb65f4fe26b5a07136db808d5b289 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0cd7bb9e2e1138b4f90d1f5ab28ce014 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e1e6eb057e584f6c5b0f75f9469a814 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6227952a851abd817472ac5105f8c8a5 |
publicationDate | 2000-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100260375-B1 |
titleOfInvention | Weather Resistant Resin Composition |
abstract | The present invention relates to a method for effectively reducing the water content in the ASA resin particles and improving the impact strength, which is a disadvantage of the ASA resin, wherein 30 to 50 parts by weight of butyl acrylate monomers and 0.1 to 4 parts of methyl meta are added to 100 parts by weight of the total monomers. A butyl acrylate rubber polymer is prepared by copolymerizing acrylate (MMA) and 0.1-6 parts of acrylonitrile (AN) at the same time, increasing the effective surface area of the rubber particles to maximize the efficiency of the butyl acrylate rubber polymer and emulsifying agent. 0.2-1.0 parts by weight of an alkyl sulfo succinate metal salt having 12 to 18 carbon atoms, an alkyl sulfate ester or a sulfonic acid metal salt having 12 to 20 carbon atoms, and a SAN (Styrene-Acrylonitrile) copolymer resin is grafted to an acrylic rubber polymer. 40 to 60 parts by weight of aromatic vinyl compound and vinyl cyanide based on 100 parts by weight of the total monomers By water 10 to 20 parts by weight of 0.5 to 3.0 and a carboxylic acid metal salt with the rosin acid metal salt and a carbon number of C 12 ~C 20 parts by weight of an emulsifier used, it is possible to reduce the moisture inside the ASA particle efficiently improve the productivity dried In addition, the present invention provides a method of significantly improving the impact strength of the ASA resin compared to the existing manufacturing method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100359875-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100384377-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20000000786-A |
priorityDate | 1997-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 85.