Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e0412713ae7ec4661e9923881f9502d |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G69-36 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-02 |
filingDate |
1997-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2000-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c93b9d9dab50759a855dc851795ce6d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2f0b0bc8c10eb93a6d00f32144a76ce |
publicationDate |
2000-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
KR-100246491-B1 |
titleOfInvention |
Method for producing polyamide polymer having excellent flexibility |
abstract |
The present invention relates to an extruded polyamide polymer having excellent flexibility, comprising 70 to 90 parts by weight of a salt consisting of hexamethylene diamine and dicarboxylic acid, and 10 to 30 parts by weight of lactam having 6 to 12 carbon atoms into the reactor. 10 to 500 ppm of sodium 2,2-methylene-bis (4,6-di-tert-butylphenyl) phosphate (C 29 H 42 O 4 PNa) was added as a nucleating agent to the composition at 0.5 to 5 hours at 230 to 280 ° C. After the reaction was carried out by heating, 5 to 25% by weight of butylbenzenesulfonamide was added as a softening agent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109575273-A |
priorityDate |
1997-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |