http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100230623-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33c922e05f6133b7d72dbb849d77487d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 |
filingDate | 1997-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1999-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7890e2f307be983e99f1b6b7b3c1d8fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87c2684089fbb7fb73d30a1cf90227bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_651b7d8c0c350bb1f0aec7b6045f91bf |
publicationDate | 1999-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-100230623-B1 |
titleOfInvention | Composition for polymerizing open cell polystyrene foam |
abstract | The present invention relates to a composition for polymerizing a low density, porous crosslinked polymer material used as a core material of a vacuum insulator, wherein polyphenylene oxide is used based on the weight of a hydrophobic vinyl monomer while a small amount of divinyl benzene, a crosslinking agent, is used. It is for increasing the mechanical strength by raising the conversion rate of the polymeric material obtained by superposition | polymerization using a weight part and more preferably 10-20 weight part mixture by 10% or more, and increasing the degree of crosslinking by crosslinking of polyphenylene oxide. |