abstract |
As described herein, 100 parts by weight of polyolefin (A) having a density of 0.930 g / cm 3 or less and a melt index of 2 g / 10 minutes or less, 100 to 400 parts by weight of a filler (B), molecular weight having an ester bond or an amide defect and a molecular weight 1 to 100 parts by weight of a plasticizer (C) composed of a compound having a boiling point of at least 100 and a boiling point of 200 ° C. or higher and 100 ° C. or lower at normal pressure, and 0.0001 to 0.1 part by weight of the radical generator (D). Resin composition, a porous film or sheet prepared therefrom, and a method for producing a porous film or sheet. |